Previous Next

ESAB

OK Tigrod 19.30

OK Tigrod 19.30
  • OK Tigrod 19.30
  • OK Tigrod 19.30

Bare copper wire for the GTAW joining of copper-zinc alloys and low-alloyed copper alloys. OK Tigrod 19.30 is alloyed with silicon and manganese and has good flow properties and wear resistance. The alloy is widely used in the joining of zinc-coated steel sheets andfor joining low- and non-alloyed steels and cast iron. OK Tigrod 19.30 is normally welded with pure Ar as the shielding gas.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 350 MPa 150 MPa

Weld Metal Analysis

MnCuZnSiSnFe
0.9 %96 %0.05 %3 %0.01 %0.05 %

Classifications: SFA/AWS A5.7, ERCuSi-A, Wire Electrode, EN ISO 24373, CuSi3Mn1, Wire Electrode

Alloy Type: Alloyed copper (Cu + 3 % Si )